The physical and electrochromic properties of Prussian Blue thin films electrodeposited on ITO electrodes

Bibliographic Details
Main Author: Isfahani, V. Bayzi
Publication Date: 2019
Other Authors: Memarian, N., Dizaji, Hamid Rezagholipour, Arab, A., Silva, Maria Manuela
Format: Article
Language: eng
Source: Repositórios Científicos de Acesso Aberto de Portugal (RCAAP)
Download full: https://hdl.handle.net/1822/72885
Summary: In this article, a set of Prussian Blue (PB) thin films with different electrodeposition times (25 s, 50 s, 75 s, 100 s and 150 s) in air at ambient temperature was prepared. The layers were characterized by a variety of techniques which include, field effect scanning electron microscopy, energy-dispersive X-ray spectrometer, X-ray diffraction, Fourier transform infared spectroscopy, UV-Vis spectrophotometry, and electrochemical analysis. A simple and exact electrochemical method was used to estimate the optimal voltages for coloring and bleaching of different PB layers. Controlling electrodeposition time along with applying suitable voltage enabled us to investigate and improve electrochromic properties of PB layer. The sample prepared under 75 s deposition time showed probably a composition intermediate between the insoluble and soluble form. Furthermore, this sample (S75) shows a better electrochromic properties. High value of electrochromic contrast 55.36% at 555 nm and well stability of ion exchange by cycling are the characteristics of this layer. The control of the deposition time resulted in an increase of 9.38 times of the contrast ratio and corresponding values for optical density (Delta OD) of the PB layers.
id RCAP_db42b4619b09a8e42a4ba37c449ca090
oai_identifier_str oai:repositorium.sdum.uminho.pt:1822/72885
network_acronym_str RCAP
network_name_str Repositórios Científicos de Acesso Aberto de Portugal (RCAAP)
repository_id_str https://opendoar.ac.uk/repository/7160
spelling The physical and electrochromic properties of Prussian Blue thin films electrodeposited on ITO electrodesElectrodepositionPrussian blueThin filmElectrochromic propertiesCiências Naturais::Ciências BiológicasScience & TechnologyIn this article, a set of Prussian Blue (PB) thin films with different electrodeposition times (25 s, 50 s, 75 s, 100 s and 150 s) in air at ambient temperature was prepared. The layers were characterized by a variety of techniques which include, field effect scanning electron microscopy, energy-dispersive X-ray spectrometer, X-ray diffraction, Fourier transform infared spectroscopy, UV-Vis spectrophotometry, and electrochemical analysis. A simple and exact electrochemical method was used to estimate the optimal voltages for coloring and bleaching of different PB layers. Controlling electrodeposition time along with applying suitable voltage enabled us to investigate and improve electrochromic properties of PB layer. The sample prepared under 75 s deposition time showed probably a composition intermediate between the insoluble and soluble form. Furthermore, this sample (S75) shows a better electrochromic properties. High value of electrochromic contrast 55.36% at 555 nm and well stability of ion exchange by cycling are the characteristics of this layer. The control of the deposition time resulted in an increase of 9.38 times of the contrast ratio and corresponding values for optical density (Delta OD) of the PB layers.The authors also acknowledgement FEDER, through COMPETE and Fundacao para a Ciencia e a Tecnologia (FCT) Pest-OE/QUI/UI0616/2014 and the project LUMECD (POCI-01-0145-FEDER-016884).ElsevierUniversidade do MinhoIsfahani, V. BayziMemarian, N.Dizaji, Hamid RezagholipourArab, A.Silva, Maria Manuela20192019-01-01T00:00:00Zinfo:eu-repo/semantics/publishedVersioninfo:eu-repo/semantics/articleapplication/pdfapplication/pdfhttps://hdl.handle.net/1822/72885eng0013-468610.1016/j.electacta.2019.02.120https://www.sciencedirect.com/science/article/pii/S0013468619303901info:eu-repo/semantics/openAccessreponame:Repositórios Científicos de Acesso Aberto de Portugal (RCAAP)instname:FCCN, serviços digitais da FCT – Fundação para a Ciência e a Tecnologiainstacron:RCAAP2025-04-12T05:26:53Zoai:repositorium.sdum.uminho.pt:1822/72885Portal AgregadorONGhttps://www.rcaap.pt/oai/openaireinfo@rcaap.ptopendoar:https://opendoar.ac.uk/repository/71602025-05-28T16:35:28.992206Repositórios Científicos de Acesso Aberto de Portugal (RCAAP) - FCCN, serviços digitais da FCT – Fundação para a Ciência e a Tecnologiafalse
dc.title.none.fl_str_mv The physical and electrochromic properties of Prussian Blue thin films electrodeposited on ITO electrodes
title The physical and electrochromic properties of Prussian Blue thin films electrodeposited on ITO electrodes
spellingShingle The physical and electrochromic properties of Prussian Blue thin films electrodeposited on ITO electrodes
Isfahani, V. Bayzi
Electrodeposition
Prussian blue
Thin film
Electrochromic properties
Ciências Naturais::Ciências Biológicas
Science & Technology
title_short The physical and electrochromic properties of Prussian Blue thin films electrodeposited on ITO electrodes
title_full The physical and electrochromic properties of Prussian Blue thin films electrodeposited on ITO electrodes
title_fullStr The physical and electrochromic properties of Prussian Blue thin films electrodeposited on ITO electrodes
title_full_unstemmed The physical and electrochromic properties of Prussian Blue thin films electrodeposited on ITO electrodes
title_sort The physical and electrochromic properties of Prussian Blue thin films electrodeposited on ITO electrodes
author Isfahani, V. Bayzi
author_facet Isfahani, V. Bayzi
Memarian, N.
Dizaji, Hamid Rezagholipour
Arab, A.
Silva, Maria Manuela
author_role author
author2 Memarian, N.
Dizaji, Hamid Rezagholipour
Arab, A.
Silva, Maria Manuela
author2_role author
author
author
author
dc.contributor.none.fl_str_mv Universidade do Minho
dc.contributor.author.fl_str_mv Isfahani, V. Bayzi
Memarian, N.
Dizaji, Hamid Rezagholipour
Arab, A.
Silva, Maria Manuela
dc.subject.por.fl_str_mv Electrodeposition
Prussian blue
Thin film
Electrochromic properties
Ciências Naturais::Ciências Biológicas
Science & Technology
topic Electrodeposition
Prussian blue
Thin film
Electrochromic properties
Ciências Naturais::Ciências Biológicas
Science & Technology
description In this article, a set of Prussian Blue (PB) thin films with different electrodeposition times (25 s, 50 s, 75 s, 100 s and 150 s) in air at ambient temperature was prepared. The layers were characterized by a variety of techniques which include, field effect scanning electron microscopy, energy-dispersive X-ray spectrometer, X-ray diffraction, Fourier transform infared spectroscopy, UV-Vis spectrophotometry, and electrochemical analysis. A simple and exact electrochemical method was used to estimate the optimal voltages for coloring and bleaching of different PB layers. Controlling electrodeposition time along with applying suitable voltage enabled us to investigate and improve electrochromic properties of PB layer. The sample prepared under 75 s deposition time showed probably a composition intermediate between the insoluble and soluble form. Furthermore, this sample (S75) shows a better electrochromic properties. High value of electrochromic contrast 55.36% at 555 nm and well stability of ion exchange by cycling are the characteristics of this layer. The control of the deposition time resulted in an increase of 9.38 times of the contrast ratio and corresponding values for optical density (Delta OD) of the PB layers.
publishDate 2019
dc.date.none.fl_str_mv 2019
2019-01-01T00:00:00Z
dc.type.status.fl_str_mv info:eu-repo/semantics/publishedVersion
dc.type.driver.fl_str_mv info:eu-repo/semantics/article
format article
status_str publishedVersion
dc.identifier.uri.fl_str_mv https://hdl.handle.net/1822/72885
url https://hdl.handle.net/1822/72885
dc.language.iso.fl_str_mv eng
language eng
dc.relation.none.fl_str_mv 0013-4686
10.1016/j.electacta.2019.02.120
https://www.sciencedirect.com/science/article/pii/S0013468619303901
dc.rights.driver.fl_str_mv info:eu-repo/semantics/openAccess
eu_rights_str_mv openAccess
dc.format.none.fl_str_mv application/pdf
application/pdf
dc.publisher.none.fl_str_mv Elsevier
publisher.none.fl_str_mv Elsevier
dc.source.none.fl_str_mv reponame:Repositórios Científicos de Acesso Aberto de Portugal (RCAAP)
instname:FCCN, serviços digitais da FCT – Fundação para a Ciência e a Tecnologia
instacron:RCAAP
instname_str FCCN, serviços digitais da FCT – Fundação para a Ciência e a Tecnologia
instacron_str RCAAP
institution RCAAP
reponame_str Repositórios Científicos de Acesso Aberto de Portugal (RCAAP)
collection Repositórios Científicos de Acesso Aberto de Portugal (RCAAP)
repository.name.fl_str_mv Repositórios Científicos de Acesso Aberto de Portugal (RCAAP) - FCCN, serviços digitais da FCT – Fundação para a Ciência e a Tecnologia
repository.mail.fl_str_mv info@rcaap.pt
_version_ 1833596039797407744