A DLC/diamond bilayer approach for reducing the initial friction towards a highbearing capacity
Main Author: | |
---|---|
Publication Date: | 2012 |
Other Authors: | , , , , , |
Format: | Article |
Language: | eng |
Source: | Repositórios Científicos de Acesso Aberto de Portugal (RCAAP) |
Download full: | https://hdl.handle.net/1822/20578 |
Summary: | Sliding contact mechanics is used to account for the net increase of the bearing capacity of high wear-resistant CVD diamond coatings when an outer layer of a DLC lubricant film is deposited on their top surface. Experimental results,namely the critical failure load, taken from reciprocating ball-on-plate tribological testing of such DLC/diamond bilayers, are on the basis of this statement. DC magnetron sputtering was used to grow thin DLC lubricant coatings (non-hydrogenated and hydrogenated varieties) on the top of CVD diamond films (microcrystalline and nanocrystalline types). The application of the von Mises maximum yield parameter (J2)1/2 criterion demonstrates to be an adequate method for designing low-friction and high-bearing capacity systems for high-demanding tribological applications. Calculation of (J2)1/2 supports that the most significant increase observed on the coatings’ bearing capacity (from 20 N to 60 N) takes place when microcrystalline diamond is coated by hydrogenated DLC that decreases the initial friction coefficient peak (from 0.76 to 0.41). |
id |
RCAP_2f11f1c71dda3ce91aaa3f9c22cc1ec3 |
---|---|
oai_identifier_str |
oai:repositorium.sdum.uminho.pt:1822/20578 |
network_acronym_str |
RCAP |
network_name_str |
Repositórios Científicos de Acesso Aberto de Portugal (RCAAP) |
repository_id_str |
https://opendoar.ac.uk/repository/7160 |
spelling |
A DLC/diamond bilayer approach for reducing the initial friction towards a highbearing capacityDLCCVD diamondTribologyContact mechanicsScience & TechnologySliding contact mechanics is used to account for the net increase of the bearing capacity of high wear-resistant CVD diamond coatings when an outer layer of a DLC lubricant film is deposited on their top surface. Experimental results,namely the critical failure load, taken from reciprocating ball-on-plate tribological testing of such DLC/diamond bilayers, are on the basis of this statement. DC magnetron sputtering was used to grow thin DLC lubricant coatings (non-hydrogenated and hydrogenated varieties) on the top of CVD diamond films (microcrystalline and nanocrystalline types). The application of the von Mises maximum yield parameter (J2)1/2 criterion demonstrates to be an adequate method for designing low-friction and high-bearing capacity systems for high-demanding tribological applications. Calculation of (J2)1/2 supports that the most significant increase observed on the coatings’ bearing capacity (from 20 N to 60 N) takes place when microcrystalline diamond is coated by hydrogenated DLC that decreases the initial friction coefficient peak (from 0.76 to 0.41).Fundação para a Ciência e a Tecnologia (FCT)ElsevierUniversidade do MinhoAmaral, M.Carreira, D. JFernandes, A. J. S.Abreu, C. S.Oliveira, F. J.Gomes, J. R.Silva, R. F.2012-06-302012-06-30T00:00:00Zinfo:eu-repo/semantics/publishedVersioninfo:eu-repo/semantics/articleapplication/pdfhttps://hdl.handle.net/1822/20578eng0043-164810.1016/j.wear.2012.05.026http://dx.doi.org/10.1016/j.wear.2012.05.026info:eu-repo/semantics/openAccessreponame:Repositórios Científicos de Acesso Aberto de Portugal (RCAAP)instname:FCCN, serviços digitais da FCT – Fundação para a Ciência e a Tecnologiainstacron:RCAAP2025-04-12T04:11:21Zoai:repositorium.sdum.uminho.pt:1822/20578Portal AgregadorONGhttps://www.rcaap.pt/oai/openaireinfo@rcaap.ptopendoar:https://opendoar.ac.uk/repository/71602025-05-28T14:54:47.103861Repositórios Científicos de Acesso Aberto de Portugal (RCAAP) - FCCN, serviços digitais da FCT – Fundação para a Ciência e a Tecnologiafalse |
dc.title.none.fl_str_mv |
A DLC/diamond bilayer approach for reducing the initial friction towards a highbearing capacity |
title |
A DLC/diamond bilayer approach for reducing the initial friction towards a highbearing capacity |
spellingShingle |
A DLC/diamond bilayer approach for reducing the initial friction towards a highbearing capacity Amaral, M. DLC CVD diamond Tribology Contact mechanics Science & Technology |
title_short |
A DLC/diamond bilayer approach for reducing the initial friction towards a highbearing capacity |
title_full |
A DLC/diamond bilayer approach for reducing the initial friction towards a highbearing capacity |
title_fullStr |
A DLC/diamond bilayer approach for reducing the initial friction towards a highbearing capacity |
title_full_unstemmed |
A DLC/diamond bilayer approach for reducing the initial friction towards a highbearing capacity |
title_sort |
A DLC/diamond bilayer approach for reducing the initial friction towards a highbearing capacity |
author |
Amaral, M. |
author_facet |
Amaral, M. Carreira, D. J Fernandes, A. J. S. Abreu, C. S. Oliveira, F. J. Gomes, J. R. Silva, R. F. |
author_role |
author |
author2 |
Carreira, D. J Fernandes, A. J. S. Abreu, C. S. Oliveira, F. J. Gomes, J. R. Silva, R. F. |
author2_role |
author author author author author author |
dc.contributor.none.fl_str_mv |
Universidade do Minho |
dc.contributor.author.fl_str_mv |
Amaral, M. Carreira, D. J Fernandes, A. J. S. Abreu, C. S. Oliveira, F. J. Gomes, J. R. Silva, R. F. |
dc.subject.por.fl_str_mv |
DLC CVD diamond Tribology Contact mechanics Science & Technology |
topic |
DLC CVD diamond Tribology Contact mechanics Science & Technology |
description |
Sliding contact mechanics is used to account for the net increase of the bearing capacity of high wear-resistant CVD diamond coatings when an outer layer of a DLC lubricant film is deposited on their top surface. Experimental results,namely the critical failure load, taken from reciprocating ball-on-plate tribological testing of such DLC/diamond bilayers, are on the basis of this statement. DC magnetron sputtering was used to grow thin DLC lubricant coatings (non-hydrogenated and hydrogenated varieties) on the top of CVD diamond films (microcrystalline and nanocrystalline types). The application of the von Mises maximum yield parameter (J2)1/2 criterion demonstrates to be an adequate method for designing low-friction and high-bearing capacity systems for high-demanding tribological applications. Calculation of (J2)1/2 supports that the most significant increase observed on the coatings’ bearing capacity (from 20 N to 60 N) takes place when microcrystalline diamond is coated by hydrogenated DLC that decreases the initial friction coefficient peak (from 0.76 to 0.41). |
publishDate |
2012 |
dc.date.none.fl_str_mv |
2012-06-30 2012-06-30T00:00:00Z |
dc.type.status.fl_str_mv |
info:eu-repo/semantics/publishedVersion |
dc.type.driver.fl_str_mv |
info:eu-repo/semantics/article |
format |
article |
status_str |
publishedVersion |
dc.identifier.uri.fl_str_mv |
https://hdl.handle.net/1822/20578 |
url |
https://hdl.handle.net/1822/20578 |
dc.language.iso.fl_str_mv |
eng |
language |
eng |
dc.relation.none.fl_str_mv |
0043-1648 10.1016/j.wear.2012.05.026 http://dx.doi.org/10.1016/j.wear.2012.05.026 |
dc.rights.driver.fl_str_mv |
info:eu-repo/semantics/openAccess |
eu_rights_str_mv |
openAccess |
dc.format.none.fl_str_mv |
application/pdf |
dc.publisher.none.fl_str_mv |
Elsevier |
publisher.none.fl_str_mv |
Elsevier |
dc.source.none.fl_str_mv |
reponame:Repositórios Científicos de Acesso Aberto de Portugal (RCAAP) instname:FCCN, serviços digitais da FCT – Fundação para a Ciência e a Tecnologia instacron:RCAAP |
instname_str |
FCCN, serviços digitais da FCT – Fundação para a Ciência e a Tecnologia |
instacron_str |
RCAAP |
institution |
RCAAP |
reponame_str |
Repositórios Científicos de Acesso Aberto de Portugal (RCAAP) |
collection |
Repositórios Científicos de Acesso Aberto de Portugal (RCAAP) |
repository.name.fl_str_mv |
Repositórios Científicos de Acesso Aberto de Portugal (RCAAP) - FCCN, serviços digitais da FCT – Fundação para a Ciência e a Tecnologia |
repository.mail.fl_str_mv |
info@rcaap.pt |
_version_ |
1833594972278882304 |