Corrosion and tribocorrosion behaviour of Ti6Al4V produced by selective laser melting and hot pressing in comparison with the commercial alloy

Bibliographic Details
Main Author: Toptan, Fatih
Publication Date: 2019
Other Authors: Alves, Alexandra Manuela Vieira Cruz Pinto, Carvalho, Oscar, Bartolomeu, Flavio, Pinto, A. M. P., Silva, Filipe Samuel, Miranda, Maria Georgina Macedo
Format: Article
Language: eng
Source: Repositórios Científicos de Acesso Aberto de Portugal (RCAAP)
Download full: https://hdl.handle.net/1822/66293
Summary: The corrosion and tribocorrosion behaviour of SLM-produced Ti6Al4V alloy was studied in comparison with its HP and commercial counterparts in 9 g/L NaClsolution at body temperature. Results showed that SLM processing route influenced the electrochemical response of the SLM-produced alloy by leading to a relatively lower quality for the passive film due to decreased beta phase and the formation of alpha' phase. However, after tribocorrosion, neither the total volume loss nor the volume loss under the influence of mechanical wear and wear accelerated corrosion showed any statistically significant difference between the processing routes.
id RCAP_043a09d3ef40bea3df64c5739c9e07c8
oai_identifier_str oai:repositorium.sdum.uminho.pt:1822/66293
network_acronym_str RCAP
network_name_str Repositórios Científicos de Acesso Aberto de Portugal (RCAAP)
repository_id_str https://opendoar.ac.uk/repository/7160
spelling Corrosion and tribocorrosion behaviour of Ti6Al4V produced by selective laser melting and hot pressing in comparison with the commercial alloyCorrosionhot pressingselective laser meltingTi6A14VtribocorrosionTi6Al4VScience & TechnologyThe corrosion and tribocorrosion behaviour of SLM-produced Ti6Al4V alloy was studied in comparison with its HP and commercial counterparts in 9 g/L NaClsolution at body temperature. Results showed that SLM processing route influenced the electrochemical response of the SLM-produced alloy by leading to a relatively lower quality for the passive film due to decreased beta phase and the formation of alpha' phase. However, after tribocorrosion, neither the total volume loss nor the volume loss under the influence of mechanical wear and wear accelerated corrosion showed any statistically significant difference between the processing routes.This study was supported by FCT with the reference project UID/EEA/04436/2013, by FEDER funds through the COMPETE 2020 - Program Operacional Competitividade e Internacionalizacao (POCI) with the reference project POCI-01-0145-FEDER-006941, together with projects NORTE-01-0145-FEDER-000018-HAMaBICo and PTDC/EMS-TEC/5422/2014. The authors would also like to acknowledge Prof. Grata Minas for the provision of the profilometry.Elsevier ScienceUniversidade do MinhoToptan, FatihAlves, Alexandra Manuela Vieira Cruz PintoCarvalho, OscarBartolomeu, FlavioPinto, A. M. P.Silva, Filipe SamuelMiranda, Maria Georgina Macedo20192019-01-01T00:00:00Zinfo:eu-repo/semantics/publishedVersioninfo:eu-repo/semantics/articleapplication/pdfhttps://hdl.handle.net/1822/66293eng0924-013610.1016/j.jmatprotec.2018.11.008info:eu-repo/semantics/openAccessreponame:Repositórios Científicos de Acesso Aberto de Portugal (RCAAP)instname:FCCN, serviços digitais da FCT – Fundação para a Ciência e a Tecnologiainstacron:RCAAP2025-04-12T04:29:18Zoai:repositorium.sdum.uminho.pt:1822/66293Portal AgregadorONGhttps://www.rcaap.pt/oai/openaireinfo@rcaap.ptopendoar:https://opendoar.ac.uk/repository/71602025-05-28T15:14:33.073944Repositórios Científicos de Acesso Aberto de Portugal (RCAAP) - FCCN, serviços digitais da FCT – Fundação para a Ciência e a Tecnologiafalse
dc.title.none.fl_str_mv Corrosion and tribocorrosion behaviour of Ti6Al4V produced by selective laser melting and hot pressing in comparison with the commercial alloy
title Corrosion and tribocorrosion behaviour of Ti6Al4V produced by selective laser melting and hot pressing in comparison with the commercial alloy
spellingShingle Corrosion and tribocorrosion behaviour of Ti6Al4V produced by selective laser melting and hot pressing in comparison with the commercial alloy
Toptan, Fatih
Corrosion
hot pressing
selective laser melting
Ti6A14V
tribocorrosion
Ti6Al4V
Science & Technology
title_short Corrosion and tribocorrosion behaviour of Ti6Al4V produced by selective laser melting and hot pressing in comparison with the commercial alloy
title_full Corrosion and tribocorrosion behaviour of Ti6Al4V produced by selective laser melting and hot pressing in comparison with the commercial alloy
title_fullStr Corrosion and tribocorrosion behaviour of Ti6Al4V produced by selective laser melting and hot pressing in comparison with the commercial alloy
title_full_unstemmed Corrosion and tribocorrosion behaviour of Ti6Al4V produced by selective laser melting and hot pressing in comparison with the commercial alloy
title_sort Corrosion and tribocorrosion behaviour of Ti6Al4V produced by selective laser melting and hot pressing in comparison with the commercial alloy
author Toptan, Fatih
author_facet Toptan, Fatih
Alves, Alexandra Manuela Vieira Cruz Pinto
Carvalho, Oscar
Bartolomeu, Flavio
Pinto, A. M. P.
Silva, Filipe Samuel
Miranda, Maria Georgina Macedo
author_role author
author2 Alves, Alexandra Manuela Vieira Cruz Pinto
Carvalho, Oscar
Bartolomeu, Flavio
Pinto, A. M. P.
Silva, Filipe Samuel
Miranda, Maria Georgina Macedo
author2_role author
author
author
author
author
author
dc.contributor.none.fl_str_mv Universidade do Minho
dc.contributor.author.fl_str_mv Toptan, Fatih
Alves, Alexandra Manuela Vieira Cruz Pinto
Carvalho, Oscar
Bartolomeu, Flavio
Pinto, A. M. P.
Silva, Filipe Samuel
Miranda, Maria Georgina Macedo
dc.subject.por.fl_str_mv Corrosion
hot pressing
selective laser melting
Ti6A14V
tribocorrosion
Ti6Al4V
Science & Technology
topic Corrosion
hot pressing
selective laser melting
Ti6A14V
tribocorrosion
Ti6Al4V
Science & Technology
description The corrosion and tribocorrosion behaviour of SLM-produced Ti6Al4V alloy was studied in comparison with its HP and commercial counterparts in 9 g/L NaClsolution at body temperature. Results showed that SLM processing route influenced the electrochemical response of the SLM-produced alloy by leading to a relatively lower quality for the passive film due to decreased beta phase and the formation of alpha' phase. However, after tribocorrosion, neither the total volume loss nor the volume loss under the influence of mechanical wear and wear accelerated corrosion showed any statistically significant difference between the processing routes.
publishDate 2019
dc.date.none.fl_str_mv 2019
2019-01-01T00:00:00Z
dc.type.status.fl_str_mv info:eu-repo/semantics/publishedVersion
dc.type.driver.fl_str_mv info:eu-repo/semantics/article
format article
status_str publishedVersion
dc.identifier.uri.fl_str_mv https://hdl.handle.net/1822/66293
url https://hdl.handle.net/1822/66293
dc.language.iso.fl_str_mv eng
language eng
dc.relation.none.fl_str_mv 0924-0136
10.1016/j.jmatprotec.2018.11.008
dc.rights.driver.fl_str_mv info:eu-repo/semantics/openAccess
eu_rights_str_mv openAccess
dc.format.none.fl_str_mv application/pdf
dc.publisher.none.fl_str_mv Elsevier Science
publisher.none.fl_str_mv Elsevier Science
dc.source.none.fl_str_mv reponame:Repositórios Científicos de Acesso Aberto de Portugal (RCAAP)
instname:FCCN, serviços digitais da FCT – Fundação para a Ciência e a Tecnologia
instacron:RCAAP
instname_str FCCN, serviços digitais da FCT – Fundação para a Ciência e a Tecnologia
instacron_str RCAAP
institution RCAAP
reponame_str Repositórios Científicos de Acesso Aberto de Portugal (RCAAP)
collection Repositórios Científicos de Acesso Aberto de Portugal (RCAAP)
repository.name.fl_str_mv Repositórios Científicos de Acesso Aberto de Portugal (RCAAP) - FCCN, serviços digitais da FCT – Fundação para a Ciência e a Tecnologia
repository.mail.fl_str_mv info@rcaap.pt
_version_ 1833595189538586624